We also Produce ICCI Rolls by sand casting technology. The hardness of these rolls varies from 55-75 shore harness. These are cast iron based rolls alloyed with Nickel, Chromium and Molybdenum having a matrix of pearlite and carbide with flake graphite. The material has very good thermal properties coupled with property of imparting good surface finish to the products.

| Hardness | C | Mn | Si | P | S | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| 55-65 | 2.50/3.20 | 0.50/0.70 | 1.50/1.70 | 0.11 MAX | 0.11 MAX | 1.00/1.80 | 0.80/1.20 | 0.20/0.30 |